| Density | 1.200 (g/㎤) |
| Hardness | 74~80 (shoreD) |
| Tensile strength | 25~30 (MPa) |
| Tensile Modulus | 2150~2370 (MPa) |
| Flexural modulus | 2650~2750 (MPa) |
| Elongation at break | 12~20 (%) |
| Impact strength | 58~68 (J/m) |
| Glass transition temperature | 55~70 (℃) |
| HDT(0.45MPa) | 60 (℃) |
| Density | 1.200 (g/㎤) |
| Hardness | 74~80 (shoreD) |
| Tensile strength | 25~30 (MPa) |
| Tensile Modulus | 2150~2370 (MPa) |
| Flexural modulus | 2650~2750 (MPa) |
| Elongation at break | 12~20 (%) |
| Impact strength | 58~68 (J/m) |
| Glass transition temperature | 55~70 (℃) |
| HDT(0.45MPa) | 60 (℃) |